Using blast furnace converter/electric furnace smelting, the slab is continuously cast, and then heated by a step heating furnace, high-pressure descaling, and multi pass hot rolling (rough rolling+precision rolling). The final rolling temperature is controlled at 850~950 ℃, and it is finally coiled into a coil with excellent plasticity and toughness.